How to print compatible bricks
Bricks only hold together if the studs are within a few hundredths of a millimetre of the right size. Every printer is a little different, so calibrate first, then print the whole set.
The models are designed to standard brick dimensions, but how well printed parts fit each other or moulded bricks depends on your printer, filament, slicer and calibration. Test a few pieces before printing a whole set.
Quick start
- 01Print the fit gauge
Download the stud fit gauge and print it with your usual settings.
- 02Find the best stud
Press a printed 2 × 2 brick (or a moulded one) onto each stud. Note the size that holds firmly but comes off by hand.
- 03Tune your slicer
Adjust XY (horizontal) compensation by half the difference between that size and 4.80 mm, then reprint one brick to check.
- 04Print the set
Download the set package. Print each STL as many times as inventory.csv says, in the colours listed.
Orientation and supports
Each part page lists the recommended orientation. These are the general rules.
- Bricks and plates: studs up
Flat on the bed, studs on top. No supports — the top surface bridges over the hollow underside.
- Slopes: studs up
A 45° face prints cleanly without supports. Steeper overhangs need them.
- Pins: on their side
Layers run along the pin, so it bends instead of snapping. Use 100% infill.
- Pins: not standing up
Standing pins split between layers the first time they are pushed into a hole.
- Beams: flat
Holes point up, so they print round and accept pins with the designed clearance.
- Fit gauge: print it first
Studs from 4.70 to 4.95 mm. The one that grips best tells you how to tune your slicer.
FDM settings
| Setting | Start with | Why |
|---|---|---|
| Nozzle | 0.4 mm | A 0.25 mm nozzle sharpens small studs but is much slower. |
| Layer height | 0.12 mm | Studs and small parts. 0.16–0.20 mm is fine for large plates and baseplates. |
| Walls | 3 perimeters | Brick walls are 1.5 mm thick, so they are almost all perimeter. |
| Top / bottom | 5 / 4 layers | Enough to close the top over the hollow underside. |
| Infill | 15–20% | Use 100% for pins, axles and anything that takes load. |
| Speed | 40–60 mm/s | Slow the outer wall to 25–30 mm/s for accurate stud diameters. |
| Seam | Rear, aligned | Keeps the seam off the studs, where a blob would make them tight. |
| Elephant-foot compensation | 0.10–0.15 mm | Flared bottom edges stop bricks stacking flush. |
| Bed adhesion | No brim | A brim on 1 × 1 parts is fine; on bricks it leaves a lip. |
Filament and materials
- PLABest place to start
Stiff, accurate and the easiest to print. Brittle for pins. Softens above about 55 °C, so do not leave models in a hot car.
- PETGTechnic parts
Tougher and more flexible, so pins and axles survive. Slightly stringy; dry it before printing.
- ABS / ASAClosest to moulded bricks
Needs an enclosure and good ventilation because of warping and fumes.
- TPU 95ASoft parts
Flexible filament for tires, rubber bands, bendy weapons and cloth like capes and sails (print cloth about 0.6 mm thin). Parts marked "Print in TPU" need it. Print slowly with retraction mostly off.
- ResinSmall, detailed parts
Very sharp detail but brittle, and it shrinks as it cures, so studs come out tight. Use a tough or ABS-like resin, wash and cure fully, and wear nitrile gloves.
Each part in a set lists a colour. Any close filament match works.
Tolerances
| Dimension | Nominal | Notes |
|---|---|---|
| Stud pitch | 8.00 mm | Distance between stud centres. Never change this. |
| Stud diameter | 4.80 mm | The gauge brackets this from 4.70 to 4.95. |
| Stud height | 1.70 mm | |
| Plate height | 3.20 mm | A brick is three plates: 9.60 mm plus studs. |
| Side clearance | 0.10 mm per face | A 2 × 4 brick is 15.8 × 31.8 mm, not 16 × 32. |
| Wall thickness | 1.50 mm | v1.1 models. v1.0 used 1.2 mm, which gripped too loosely on most printers. |
| Tube outer diameter | 6.51 mm | Grips the studs from inside 2-wide parts. |
| Pin hole | 4.90 mm | With a 6.2 mm counterbore 0.8 mm deep. |
Too tight? Lower XY compensation by 0.02–0.05 mm, check for elephant foot, and make sure the seam is not on the studs. Too loose? Raise it, or print slower and slightly cooler so walls stay crisp.
Resin printing
- Angle bricks 30–45° with light supports on the underside edges, never on the studs.
- Hollow parts can trap resin. Drain them properly, or add drain holes in the tube area.
- Resin shrinks as it cures. Scale XY by about +0.5% or reduce exposure if studs are tight.
- Standard resin is brittle. Tough or ABS-like resin survives repeated assembly much better.
- Wash, then fully post-cure before handling. Uncured resin irritates skin: wear gloves and ventilate the room.
Safety
- Small parts are a choking hazard. Keep printed bricks away from children under 3.
- Home-printed parts are not safety-tested toys. Check them for sharp edges and cracks.
- Do not leave printers unattended for long jobs, and follow the filament maker’s temperature range.
- BRICKPRINT models are compatible designs, not genuine LEGO® elements. LEGO® is a trademark of the LEGO Group, which does not sponsor, authorize or endorse this site.